ASTM A333 Seamless and Welded Steel Pipe
HOME Products ABOUT US Projects SERVICE BLOG & NEWS Contact Us Español Français Türkçe Português بالعربية English
ASTM A333 Seamless and Welded Steel Pipe
Home > BLOG & NEWS > Seamless Steel Pipe
Back

ASTM A333 Seamless and Welded Steel Pipe

Date:2019-08-21    View:3108  Tags:ASTM A333 Seamless and Welded Steel Pipe

Welcome to inquiry,Emailsales@united-steel.com

Click to read the details of the product.:

1.Seamless Steel Pipe

2.Welded steel pipe

3.Oil Country Tubular Goods

4.Alloy Steel Pipe

5.Stainless Steel Products

6.Galvanized Steel Pipe

7.Pipe Fittings and Flange

8.Structural Steel Section

9.Coated Carbon Steel Pipe

ASTM A333 is the Standard Specification for Seamless and Welded Steel Pipe for Low-Temperature Service.



ASTM A333 alloy pipe shall be made by the seamless or welding process with the addition of no filler metal in the welding operation. All seamless and welded pipes shall be treated to control their microstructure. 


Seamless and Welded Steel Pipe for Low-Temperature Service.


Standards: ASTM A333/333M (ASME SA333/SA333M)

Size (mm):

Application: Seamless and Welded Steel Pipe for Low-Temperature Service.
Steel grade: Grade 1, Grade 6 .

Packing: Bare packing/bundle packing/crate packing/wooden protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.

Inspection and Test: Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength,Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test), Surface and Dimension Test,No-destructive Test, Hydrostatic Test.

Surface treatment: Oil-dip, Varnish, Passivation, Phosphating, Shot Blasting. Both ends of each crate will indicate the order no., heat no., dimensions, weight and bundles or as requested.

 Mechanical requiremnts of ASTM A333 alloy pipe

Grade Tensile Strength (MPa) Yield Point (MPa) Elongation (%)
Y X
Grade 1 ≥380 ≥205 ≥35 ≥25
Grade 3 ≥450 ≥240 ≥30 ≥20
Grade 4 ≥415 ≥240 ≥30 ≥16.5
Grade 6 ≥415 ≥240 ≥30 ≥16.5
Grade 7 ≥450 ≥240 ≥30 ≥22
Grade 8 ≥690 ≥515 ≥22
Grade 9 ≥435 ≥315 ≥28
Grade 10 ≥550 ≥450 ≥22
Grade 11 ≥450 ≥240 ≥18
 Chemical Composition (%) of ASTM A333 steel pipe
Grade Chemical Composition (%)
C Si Mn P S Cr Ni Cu Mo V Al
Grade 1 ≤0.30 0.40-1.06 ≤0.025 ≤0.025
Grade 3 ≤0.19 0.18-0.37 0.31-0.64 ≤0.025 ≤0.025 3.18-3.82
Grade 4 ≤0.12 0.18-0.37 0.50-1.05 ≤0.025 ≤0.025 0.44-1.01 0.47-0.98 0.40-0.75 0.04-0.30
Grade 6 ≤0.30 ≥0.10 0.29-1.06 ≤0.025 ≤0.025
Grade 7 ≤0.19 0.13-0.32 ≤0.90 ≤0.025 ≤0.025 2.03-2.57
Grade 8 ≤0.13 0.13-0.32 ≤0.90 ≤0.025 ≤0.025 8.40-9.60
Grade 9 ≤0.20 0.40-1.06 ≤0.025 ≤0.025 1.60-2.24 0.75-1.25
Grade 10 ≤0.20 0.10-0.35 1.15-1.50 ≤0.03 ≤0.015 ≤0.15 ≤0.25 ≤0.015 ≤0.50 ≤0.12 ≤0.06
Grade 11 ≤0.10 ≤0.35 ≤0.6 ≤0.025 ≤0.025 ≤0.50 35.0-37.0 ≤0.50
Strike temperature condition:
Crade The lowest temperature for strike test
ASTM A333 Grade 1 -50 -45
ASTM A333 Grade 3 -150 -100
ASTM A333 Grade 4 -150 -100
ASTM A333 Grade 6 -50 -45
ASTM A333 Grade 7 -100 -75
ASTM A333 Grade 8 -320 -195
ASTM A333 Grade 9 -100 -75
ASTM A333 Grade 10 -75 -60

Delivery Condition: Normalized and Tempered
[Back]
related post
COPYRIGHT © 2016 ~ 2022 UNITED STEEL INDUSTRY CO., LTD, all rights reserved. www.united-steel.com
We use cookies and other tracking technologies to improve your browsing experience on our website, to show you personalized content and targeted ads, to analyze our website traffic, and to understand where our visitors are coming from.