Tubo galvanizado por inmersión en caliente
Tubería de acero pre galvanizada
Tubo de acero de aleación transparente
Tubería de acero de aleación soldada
Tubería soldada de acero inoxidable
Superficie: aceitada y pintada de negro para evitar la oxidación.
Grade |
UN |
C≤ |
Mn |
P≤ |
S≤ |
Si≤ |
Cr |
Mo |
Sequiv. |
||||||||
P1 |
K11522 |
0.10~0.20 |
0.30~0.80 |
0.025 |
0.025 |
0.10~0.50 |
– |
0.44~0.65 |
P2 |
K11547 |
0.10~0.20 |
0.30~0.61 |
0.025 |
0.025 |
0.10~0.30 |
0.50~0.81 |
0.44~0.65 |
P5 |
K41545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
4.00~6.00 |
0.44~0.65 |
P5b |
K51545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.00~2.00 |
4.00~6.00 |
0.44~0.65 |
P5c |
K41245 |
0.12 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
4.00~6.00 |
0.44~0.65 |
P9 |
S50400 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50~1.00 |
8.00~10.00 |
0.44~0.65 |
P11 |
K11597 |
0.05~0.15 |
0.30~0.61 |
0.025 |
0.025 |
0.50~1.00 |
1.00~1.50 |
0.44~0.65 |
P12 |
K11562 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
0.80~1.25 |
0.44~0.65 |
P15 |
K11578 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.15~1.65 |
– |
0.44~0.65 |
P21 |
K31545 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
2.65~3.35 |
0.80~1.60 |
P22 |
K21590 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
1.90~2.60 |
0.87~1.13 |
P91 |
K91560 |
0.08~0.12 |
0.30~0.60 |
0.02 |
0.01 |
0.20~0.50 |
8.00~9.50 |
0.85~1.05 |
P92 |
K92460 |
0.07~0.13 |
0.30~0.60 |
0.02 |
0.01 |
0.5 |
8.50~9.50 |
0.30~0.60 |
Requisitos de tracción
Tensile Strength, min., psi |
P-5 |
P-9 |
P-11 |
P-22 |
P-91 |
ksi |
60 |
60 |
60 |
60 |
85 |
MPa |
415 |
415 |
415 |
415 |
585 |
Yield Strength, min., psi |
|
|
|
|
|
ksi |
30 |
30 |
30 |
30 |
60 |
MPa |
205 |
205 |
205 |
205 |
415 |
Propiedades mecánicas
Mechanical properties |
P1,P2 |
P12 |
P23 |
P91 |
P92,P11 |
P122 |
Tensile strength |
380 |
415 |
510 |
585 |
620 |
620 |
Yield strength |
205 |
220 |
400 |
415 |
440 |
400 |
También mejora la resistencia a la corrosión del acero e inhibe las picaduras. El cromo (o cromo) es el componente esencial del acero inoxidable. Cualquier acero con 12% o más de cromo se considera inoxidable. El cromo es prácticamente insustituible para resistir la oxidación a temperaturas elevadas. El cromo aumenta la tracción, el rendimiento y la dureza a temperatura ambiente. La composición del tubo de acero de aleación de cromo-molibdeno lo hace ideal para su uso en plantas de energía, refinerías, plantas petroquímicas y servicios de campos petroleros donde los fluidos y gases se transportan a temperaturas y presiones extremadamente altas.
Requisitos de tratamiento térmico
Grade |
Heat Treatment Type |
Normalizing Temperature Range F [C] |
Subcritical Annealing or Tempering |
P5, P9, P11, and P22 |
Temperature Range F [C] |
||
A335 P5 (b,c) |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1250 [675] |
|
Subcritical Anneal (P5c only) |
***** |
1325 – 1375 [715 - 745] |
A335 P9 |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1250 [675] |
A335 P11 |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1200 [650] |
A335 P22 |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1250 [675] |
A335 P91 |
Normalize and Temper |
1900-1975 [1040 - 1080] |
1350-1470 [730 - 800] |
|
Quench and Temper |
1900-1975 [1040 - 1080] |
1350-1470 [730 - 800] |
Pruebas mecánicas especificadas
Prueba de tensión transversal o longitudinal y prueba de aplanamiento, prueba de dureza o prueba de flexión
Para material tratado térmicamente en un horno tipo discontinuo, las pruebas se realizarán en el 5% de la tubería de cada lote tratado. Para lotes pequeños, se deberá ensayar al menos una tubería.
Para el material tratado térmicamente mediante el proceso continuo, las pruebas se realizarán en un número suficiente de tubos para constituir el 5% del lote, pero en ningún caso menos de 2 tubos.
Notas para la prueba de dureza:
P91 no deberá tener una dureza que no exceda 250 HB/265 HV [25HRC].
Notas para la prueba de flexión:
Para tuberías cuyo diámetro exceda NPS 25 y cuya relación entre diámetro y espesor de pared sea 7.0 o menos, se deberán someter a la prueba de flexión en lugar de la prueba de aplanamiento.
A otras tuberías cuyo diámetro sea igual o superior a NPS 10 se les puede realizar la prueba de flexión en lugar de la prueba de aplanamiento, sujeto a la aprobación del comprador.
Las muestras de prueba de flexión se deben doblar a temperatura ambiente hasta 180° sin agrietarse en el exterior de la parte doblada.
Examen HIDROSTATICO
El diámetro interior del doblez será de 1 pulgada [25 mm].
Cada tramo de tubería deberá someterse a pruebas hidráulicas; como opción de fabricación, se pueden utilizar pruebas eléctricas no destructivas.